MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
American Computer Optics 12.1in Tempered LCD Glass
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Maximum Size: 8.2" X 10.6"
Abrasion: MIL-C-675C, section 4.5.11
Adhesion: MIL-C-48497A, para 4.5.3.1
Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exposure (50 C, 95% humidity)
Solubility: The coated optical surface will show no signs of deterioration after a 24 hour immersion or exposure at room temperature (-60 F to + 90F) in each of the following solutions: Distilled Water - Acetone - Ethyl Alcohol - Isopropyl Alcohol - Trichloroethylene - 1.1.1 Trichlorethane
Tempering: ATSM C1048-976

Information provided by American Computer Optics.

Key Words: optics, reflectance, anti-reflective, UV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 3000 microns
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 98 %
IR Transmittance 70 %
@Wavelength 780 - 2500 nm
Near IR
UV Transmittance 47 %
@Wavelength 300 - 380 nm
Reflection Coefficient, Visible (0-1) <= 0.010
 
Component Elements PropertiesOriginal ValueComments
Other <= 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Computer Optics 10.4in Tempered LCD Glass
American Computer Optics 15in Tempered LCD Glass
Borosilicate Glass
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
ASTM A439 Austenitic Ductile Iron type D2

CGLACO20 / 926

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.