MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled

Material Notes: Product description: Grivory HTM-4H1 is a 40 % mineral reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/6I. Acc. to ASTM: PPA, Polyphthalamide Grivory HTM-4H1 is used for injection molding technical parts. Properties are almost isotropic and strength is outstanding compared to other mineral filled materials. The main distinguishing feature of Grivory HT, when compared to other polyamides, is its good performance values at high temperatures providing parts which are stiffer, stronger and have better heat distortion stability and chemical resistance. Grivory HT is suitable for production of technical parts in the application fields of:
  • Electro
  • Electronics
  • Automotive
  • Mechanical engineering

Information provided by EMS Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³Dry; ISO 1183
Water Absorption 3.5 %3.5 %Sim. to ISO 62
Moisture Absorption 1.50 %1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 260 MPa37700 psiDry; ISO 2039-1
 260 MPa37700 psiConditioned; ISO 2039-1
Tensile Strength at Break 105 MPa15200 psiDry; ISO 527-1/-2
 105 MPa15200 psiConditioned; ISO 527-1/-2
Elongation at Break 1.5 %1.5 %Dry; ISO 527-1/-2
 1.5 %1.5 %Conditioned; ISO 527-1/-2
Tensile Modulus 7.50 GPa1090 ksiDry; ISO 527-1/-2
 7.50 GPa1090 ksiConditioned; ISO 527-1/-2
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eU
 2.50 J/cm²
@Temperature -30.0 °C
11.9 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Dry; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmDry; IEC 60093
 1.00e+11 ohm-cm1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohm1.00e+11 ohmIEC 60093
Dielectric Strength 32.0 kV/mm813 kV/inDry; IEC 60243-1
 32.0 kV/mm813 kV/inConditioned; IEC 60243-1
Comparative Tracking Index 575 V575 VConditioned; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 325 °C617 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 140 °C284 °FLong Term; ISO 2578
 270 °C518 °FShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 145 °C293 °FISO 75-1/-2
Deflection Temperature at 8.0 MPa 115 °C239 °FISO 75-1/-2
Flammability, UL94 HBHBIEC 60695-11-10
 
Descriptive Properties
AutomotiveFuel systems
 Interior
 Powertrain and Chassis
FormGranules
Industry & Consumer goodsHousewares
 Hydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
Special CharacteristicsImproved heat resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
ExxonMobil Mobilgrease HTM
KEP Kepital® F20-52G Acetal Copolymer, Low Gloss UV & Weather Resistance Grade
KEP Kepital® F30-52G Acetal Copolymer, UV & Weather Resistance Grade
Solvay HTM® 552 Bismaleimide Resin

PGRH393 / 157102

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.