MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Syensqo (Solvay Specialty Polymers) Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properties than many unreinforced thermoplastic polyester and nylon resins especially after exposure to humid environments.

These materials were specifically designed for automotive electrical and electronic applications such as connectors, sockets, and sensors. Additional applications include fuel systems where both the high elongation/ductility and superior low permeation performance to automotive fuels are needed.

They can be processed readily using conventional injection molding equipment and methods.

Information provided by Solvay Advanced Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccISO 1183A
 1.10 g/cc1.10 g/ccASTM D792
Moisture Absorption at Equilibrium 0.50 %0.50 %24 hours; ASTM D570
Linear Mold Shrinkage 0.020 cm/cm0.020 in/in93°C; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiISO 527
Tensile Strength, Yield 57.0 MPa8270 psiISO 527
 61.0 MPa8850 psiASTM D638
Elongation at Break 15 %15 %ISO 527
Elongation at Yield 5.0 %5.0 %ISO 527
 30 %30 %ASTM D638
Tensile Modulus 2.30 GPa334 ksiASTM D638
 2.30 GPa334 ksiISO 527
 0.500 GPa
@Temperature 100 °C
72.5 ksi
@Temperature 212 °F
ISO 527
Flexural Strength 65.0 MPa9430 psiISO 178
 92.0 MPa13300 psiASTM D790
 9.00 MPa
@Temperature 100 °C
1310 psi
@Temperature 212 °F
ISO 178
Flexural Modulus 1.80 GPa261 ksiISO 178
 2.10 GPa305 ksiASTM D790
 0.400 GPa
@Temperature 100 °C
58.0 ksi
@Temperature 212 °F
ISO 178
Shear Strength 53.0 MPa7690 psiASTM D732
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
Izod Impact, Unnotched NBNBASTM D4812
Izod Impact, Notched (ISO) 14.0 kJ/m²6.66 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
Dynatup @ -18°C 54.0 J39.8 ft-lbTotal Energy. Dry as molded. No temperature indicated.; D3763
Dynatup @ -18°C Max Load 454000 g1000 lbNo temperature indicated.; D3763
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.90e+15 ohm-cm3.90e+15 ohm-cmASTM D257
Surface Resistance 3.80e+15 ohm3.80e+15 ohmASTM D257
Dielectric Constant  3.2
@Frequency 60 Hz
3.2
@Frequency 60 Hz
ASTM D150
 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm432 kV/inASTM D149
Dissipation Factor  0.0040
@Frequency 60 Hz
0.0040
@Frequency 60 Hz
ASTM D150
 0.016
@Frequency 1e+6 Hz
0.016
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index >= 600 V>= 600 VASTM D3638
High Voltage Arc-Tracking Rate, HVTR 4.20 mm/min0.165 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 300 °C572 °FISO 11357-3
 300 °C572 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C183 °FISO 75Af
 185 °C365 °FASTM D648
Flammability, UL94 HBHB
Shrinkage 1.9 %1.9 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grivory® HTM-4H1 PA6T/6I-MD40
Syensqo (Solvay Specialty Polymers) Amodel® AT-5001 Polyphthalamide (PPA) Resin, at 50% RH
Syensqo (Solvay Specialty Polymers) Amodel® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
Hexcel® HexPly® F652 Bismaleimide Resin

PSOLVT88 / 21384

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.