MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: EX3 (HM 5010 T2N) is a natural colored high density polyethylene with Butene-1 as comonomer. The product is classified as PE 80 and good stress crack resistance properties combined with good impact strength.

Applications: pipe extrusion PE80 class, pressure pipe, drinking water and gas pipes, sewer pipes and their fittings, discharge pipes, for injection molded and other fittings, sheets.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccISO 1183
Melt Flow 0.45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Tensile Strength, Yield 22.0 MPaISO 527-1
Elongation at Yield 8.0 %ISO 527-1
Tensile Modulus 850 MPaISO 527-1
Charpy Impact, Notched 12.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 67.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 136 °C
 190 - 220 °C
 
Descriptive Properties
Hydrostatic Strength, hr100080°C; ISO 1167/DIN8075
MRS Classification, MPa8ISO/TR9080

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) Arak EX3 HDPE
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene
Iran Petrochemical (PCC) EX 5 HM 9450 F High Density Polyethylene
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene

PIPC241 / 149703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.