MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin.

Applications: pipe extrusion PE 80 class, industrial and pressure pipe , gas pipe, drinking water pipe, relining , fittings.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ISO 1183
Environmental Stress Crack Resistance 50 hour
@Pressure 4.00 MPa
50 hour
@Pressure 580 psi
ISO CD 16770
Melt Flow  0.45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.45 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength at Break 35.0 MPa5080 psiISO 527
Tensile Strength, Yield 22.0 MPa3190 psiISO 527
Elongation at Break >= 850 %>= 850 %ISO 527
Elongation at Yield 8.0 %8.0 %ISO 527
Tensile Modulus 0.850 GPa123 ksiISO 527
Charpy Impact, Notched 2.30 J/cm²10.9 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Softening Point 67.0 °C153 °FISO 306
Brittleness Temperature >= -80.0 °C>= -112 °FASTM D746-72
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 220 °C374 - 428 °F
 
Descriptive Properties
Flexural Creep Modulus (MPa)9504 point, 1 min; DIN 19537-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EX3 HM 5010 T2N High Density Polyethylene
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene
Iran Petrochemical (PCC) Arak EX3 HDPE
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene
Iran Petrochemical (PCC) LF0200 Low Density Polyethylene

PIPC242 / 149704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.