MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Linear Mold Shrinkage, Flow 0.012 - 0.015 cm/cm0.012 - 0.015 in/in
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm0.012 - 0.015 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 15.0 MPa2180 psi
Elongation at Break  20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
 >= 100 %
@Temperature 60.0 °C
>= 100 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
Elongation at Yield  5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
 >= 10 %
@Temperature 60.0 °C
>= 10 %
@Temperature 140 °F
 >= 10 %
@Temperature 90.0 °C
>= 10 %
@Temperature 194 °F
Tensile Modulus  0.500 GPa
@Temperature 90.0 °C
72.5 ksi
@Temperature 194 °F
 0.800 GPa
@Temperature 60.0 °C
116 ksi
@Temperature 140 °F
 1.80 GPa
@Temperature 23.0 °C
261 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -20.0 °C
9.52 ft-lb/in²
@Temperature -4.00 °F
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Charpy Impact, Notched  0.0800 J/cm²
@Temperature -20.0 °C
0.381 ft-lb/in²
@Temperature -4.00 °F
 0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C230 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °F
Vicat Softening Point 100 °C
@Load 5.00 kg
212 °F
@Load 11.0 lb
Flammability, UL94  V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Oxygen Index 33 %33 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
Glow Wire Ignition Temperature  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
 825 °C
@Thickness 2.00 mm
1520 °F
@Thickness 0.0787 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
176 - 194 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latene® AG3H2W G/30-V0E PP Homopolymer, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant
Overview of materials for Polypropylene, Mineral Reinforced
Overview of materials for Polypropylene, Flame Retardant
CENTROPLAST CENTROLEN PP-H Polypropylene homopolymer

PLATH9764 / 177460

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.