Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Low smoke density and low toxicity index. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Information provided by Lati Industria Termoplastici S.p.A. |