MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 8622 Steel, heat treated, machined to 13.7 mm rounds, pseudocarburized, 820°C (1510°F) reheat, 150°C (300°F) temper
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 8000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalize 925°C (1700°F) in 32 mm rounds, machine to 13.7 mm rounds, pseudocarburize at 925°C (1700°F) for 8 hours, box cooled to room temperature, 820°C reheat, oil quench, 150°C (300°F) temper, tested in 12.8 mm rounds

Key Words: B.S. 805 A 20, UNS G86220, ASTM A322, ASTM A331, SAE J404, SAE J770, DIN 1.6543
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 415415
Hardness, Knoop 446446Converted from Brinell
Hardness, Rockwell B 103103Converted from Brinell
Hardness, Rockwell C 4545Converted from Brinell
Hardness, Vickers 440440Converted from Brinell
Tensile Strength, Ultimate 1451 MPa210500 psi
Tensile Strength, Yield 1041 MPa
@Strain 0.2 %
151000 psi
@Strain 0.2 %
Elongation at Break 13 %13 %in 50 mm
Modulus of Elasticity 205 GPa29700 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 65 %65 %hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000234 ohm-cm0.0000234 ohm-cmTypical steel
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.475 J/g-°C0.114 BTU/lb-°FTypical steel
Thermal Conductivity 46.6 W/m-K323 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.20 - 0.25 %0.20 - 0.25 %
Chromium, Cr 0.40 - 0.60 %0.40 - 0.60 %
Iron, Fe 96.925 - 98 %96.925 - 98 %As remainder
Manganese, Mn 0.70 - 0.90 %0.70 - 0.90 %
Molybdenum, Mo 0.15 - 0.25 %0.15 - 0.25 %
Nickel, Ni 0.40 - 0.70 %0.40 - 0.70 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4718 Steel, pseudocarburized and oil quenched, 150°C (300°F) temper, 13.7 mm round
AISI 4718 Steel, pseudocarburized, reheated to 765°C (1700°F) and oil quenched, 150°C (300°F) temper, 25 mm round
AISI 6150 Steel, annealed, 25 mm (1 in.) round
AISI 8620 Steel, double quenched and tempered (150°C (300°F)), carburized
AISI 8822 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, 820°C (1510°F) reheat, 150°C (300°F) temper

M862DI / 8366

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.