MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Total 46060 UV High Density Polyethylene - Large Part Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Polyethylene: High molecular weight, high density large part blow molding resin.

Characteristics:

  • Good melt strength
  • Good impact and creep resistance
  • Excellent stress cracking resistance
  • Excellent stacking strength
  • Good rigidity
  • ASTM D 1248 - Type III, Class A, Category 5
  • ASTM D 4976-89-PE235
  • FDA Compliant

Applications:

  • Shipping containers
  • Industrial chemical tanks
  • Intermediate bulk containers
  • Agricultural chemical tanks

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.946 g/ccASTM D792
ESCR 100% Igepal® >= 1000 hourF50; ASTM D1693
ESCR 10% Igepal® >= 1000 hourF50; ASTM D1693
Melt Flow 6.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5340 psiASTM D638
Tensile Strength, Yield 3580 psiASTM D638
Elongation at Break 630 %ASTM D638
Flexural Modulus 117700 psi
@Strain 0.4 %
ASTM D790
Izod Impact, Notched 10.5 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 255 °FASTM D3417
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 440 °FBlow Molding Stock Temp.
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H6007JU High Density Polyethylene Injection Molding
A. Schulman POLYFORT™ FPP 1603 Glass Reinforced Copolymer
Bayport Polymers Baystar™ B5845 High Density Polyethylene - Blow Molding Resin
Chevron Phillips Marlex® EHM 6007 High Density Polyethylene
Dow DOWLEX™ IP-10262 High Density Polyethylene

PTOTAL739 / 130464

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.