MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SCG Chemicals EL-Lene™ H6007JU High Density Polyethylene Injection Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Key Characteristics:
  • Good processability
  • High rigidity
  • High impact resistance
  • Good weathering resistance (UV stabilizer)

Recommended Applications:

  • Crates for soft drink, bottles, pallet, garbage bins, containers
  • Industrial parts for outdoor uses such as motorcycle fenders

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.964 g/cc0.964 g/ccASTM D1505
Environmental Stress Crack Resistance 4.0 hour
@Temperature 50.0 °C
4.0 hour
@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Linear Mold Shrinkage, Flow 0.0155 cm/cm
@Thickness 2.00 mm
0.0155 in/in
@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.0096 cm/cm
@Thickness 2.00 mm
0.0096 in/in
@Thickness 0.0787 in
TPE Method
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6868ASTM D2240
Tensile Strength at Break 30.0 MPa4350 psiASTM D638
Tensile Strength, Yield 30.4 MPa4410 psiASTM D638
Elongation at Break 1000 %1000 %ASTM D638
Flexural Modulus 1.32 GPa192 ksiASTM D790
Izod Impact, Notched >= 0.343 J/cm
@Temperature 23.0 °C
>= 0.643 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 133 °C271 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total 46060 UV High Density Polyethylene - Large Part Blow Molding Resin
Dow HDPE 25455N High Density Polyethylene
ExxonMobil Paxon™ BA46-055 Blow Molding Resin
LyondellBasell Alathon® H5618 High Density Polyethylene
Kotec Carbotex K-20 Polycarbonate, General Purpose

PSCGC913 / 120667

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.