MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ExxonMobil Paxon™ BA46-055 Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Product Description: BA46-055 is a high molecular weight high density polyethylene copolymer. It possesses a combination of excellent processability, outstanding melt strength, high impact strength, chemical resistance and high stress cracking resistance. It is often used in coex applications.

Availability: Latin America, North America and South America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Automotive Fuel Tanks
  • Compression Moldings
  • Drums
  • Food packaging
  • Heavy Gauge Sheet
  • Intermediate Bulk Containers
  • Large Part Blow Molding
  • Portable Fuel Tanks
  • Small Engine Fuel Tanks
  • Thermoformed Parts
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ASTM D4883
ESCR 100% Igepal® >= 1000 hour>= 1000 hourASTM D1693 Condition B
Melt Flow 5.5 g/10 min5.5 g/10 min190 / 21.6 (HLMI); ASTM D1238
 <= 0.10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
<= 0.10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.1 MPa3500 psiASTM D638
Elongation at Break 1100 %1100 %ASTM D638
Flexural Modulus 1.03 GPa150 ksiMethod1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 420 kJ/m²200 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 127 °C260 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 °C400 °F
 
Descriptive Properties
FeaturesThermal Stabilizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total MS201 BN-NA High Density Polyethylene - Fuel Tank Resin
Dow HDPE 25455N High Density Polyethylene
ExxonMobil Paxon™ 7003 Crosslinkable Rotational Molding Resin
LyondellBasell Alathon® H5618 High Density Polyethylene
SCG Chemicals EL-Lene™ H6007JU High Density Polyethylene Injection Molding

PEXB102 / 37407

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.