MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ Vertex Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel; Air-Hardening Steel

Material Notes: TLS Vertex tool steel is a versatile, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, chromium-rich alloy carbides in the microstructure. These carbides provide good resistance to wear from sliding contact with other metals and abrasive materials. The primary alloy carbides in Vertex are smaller than the large chromium-rich alloy carbides which are characteristic of D2 tool steel. These smaller carbides result in better impact toughness and superior fatigue properties compared to D2. The molybdenum addition in Vertex enhances the hardness of the alloy carbides, and more significantly, provides superior secondary hardening response compared to D2. Therefore, unlike D2, Vertex can be tempered at higher tempering temperatures yet still attain a hardness in excess of 60 Rockwell C. Because of the higher secondary hardness, Vertex exhibits superior wear resistance compared to D2 tempered at the higher tempering temperatures, as well as the super

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.68 g/cc
Density 0.277 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 63.5Air Cooled from 1052°C, 45 minutes
 64.5Air Cooled from 1010°C, 45 minutes
 64.5Air Cooled from 1030°C, 45 minutes
Modulus of Elasticity 30000 ksi
Machinability 65 - 70 %1% Carbon Steel
Izod Impact Unnotched 22.0 ft-lbFor 63 HRC
 45.0 ft-lbFor 54 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 µm/m-°C
@Temperature 38.0 - 200 °C
 13.2 µm/m-°C
@Temperature 38.0 - 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.0 %
Chromium, Cr 8.25 %
Iron, Fe 86.6 %
Manganese, Mn 0.50 %
Molybdenum, Mo 2.25 %
Silicon, Si 1.0 %
Vanadium, V 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm BÖHLER K340 ISODUR® Premium Cold Work Steel
Latrobe LSS™ D2 Tool Steel (ASTM D2)
Chloroform (CHCl3; trichloromethane)
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel
AK Steel 410S Ferritic Stainless steel

NTIMK111 / 19458

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.