MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil Aero HFA
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with excellent low temperature properties, good anti-wear performance, and good chemical stability. Mobil Aero HFA and HF are composed of mineral base oil stock and contain shear-stable VI improvers; Mobil Aero HFS is a synthetic polyalphaolefin-based fluid.

Mobil Aero HFA is a premium quality fluid that meets the requirements of the U.S. Military specification MIL-H-5606A (now obsolete). It has a very high VI and is suitable for use at temperatures down to -54 ºC (-65 ºF). While this quality fluid is no longer used by the U.S. Military, it is still used in some older, small private, and commercial aircraft. It is also used in industrial and commercial equipment requiring good fluidity at very low temperatures, where Mobil Aero HFA provides long, trouble-free service over a wide range of operating conditions. Mobil Aero HF is a premium quality fluid that is approved against the most current version of U.S. Military specification MIL-PRF-5606. It has physical properties very similar to Mobil Aero HFA, and also meets "super-clean" requirements required by modern aircraft hydraulic systems. It is intended primarily for military aircraft, but it is also used as a hydraulic fluid for small private and commercial aircraft, and as a strut fluid in landing gear of large commercial aircraft. It is a NATO Code Number H-515 fluid. Mobil Aero HFS is a synthetic polyalphaolefin lubricant that is approved against the most current version of U.S. Military specification MIL-PRF-83282. It does not contain a viscosity index (VI) improver. It is designed for use at temperatures down to -40ºC (-40ºF). It provides lower flammability and volatility and improved stability, but has a higher viscosity at low temperature then Mobil Aero HF. It meets the "super-clean" requirements. It is intended primarily for U.S. military aircraft.It is a NATO Code Number H-537 fluid.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.882 g/ccASTM D4052
API Gravity 29 °
Viscosity Measurement 370Index; ASTM D2270
Viscosity Measure 10.4 cSt
@Temperature 54.4 °C
ASTM D445
 450 cSt
@Temperature -40.0 °C
Kinematic Viscosity; ASTM D445
 1950 cSt
@Temperature -54.0 °C
Kinematic Viscosity; ASTM D445
Kinematic Viscosity at 40°C (104°F) 13.9 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 5.1 cStASTM D445
Evaporation Loss 11 %6.5 hr @ 205°C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.040
 
Mechanical PropertiesOriginal ValueComments
Bulk Modulus 1.379 GPaIsothermal secant at 40°C, 4000 psig
Four Ball Wear 0.800 mm40 kg, 75°C, 1200 rpm; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -66.0 °CASTM D97
Flash Point 108 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.0040 %
 
Descriptive Properties
Colorred
Copper Strip Corrosion, ASTM D1302E72 hrs @ 135°C
Foam Sequence I, ASTM D113830/0
Low Temperature Stabilitypass72 hrs @ -54°C
Oxidation Corrosion Stabilitypass168 hrs @ 135°C
Rubber Swell, %19 to 30Nitrile Rubber, 168 hr @ 70°C
Sonic Shear Stability, KV change %15 (max)@ 40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Mobil Aero HF
Eastman Skydrol® 500B-4 Fire Resistant Hydraulic Fluid
Eastman Skydrol® 5 Fire Resistant Hydraulic Fluid
Dow HIGH VACUUM GREASE
ChevronTexaco TEGRA® Synthetic Barrier Fluid

WEXXON350 / 75775

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.