MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Skydrol® 5 Fire Resistant Hydraulic Fluid
Categories: Fluid

Material Notes: Product Description: Introduced in 1996, Skydrol 5 was the first Type V fluid qualified under the Boeing BMS 3-11 specification. Skydrol 5 offers higher temperature capability than Type IV fluids, the lowest density, and better paint compatibility. Skydrol 5 does not have universal air frame manufacturer approval, so consult Eastman's Skydrol Technical Service (800-260-4150) for specific approval and application information.

Application/Uses:

  • Aviation hydraulic systems

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 - 0.980 g/cc0.0350 - 0.0354 lb/in³
Viscosity Measure  3.01 - 3.41 cSt
@Temperature 99.0 °C
3.01 - 3.41 cSt
@Temperature 210 °F
 9.0 - 9.84 cSt
@Temperature 38.0 °C
9.0 - 9.84 cSt
@Temperature 100 °F
 <= 2600 cSt
@Temperature -54.0 °C
<= 2600 cSt
@Temperature -65.2 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.10<= 0.10[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Pour Point <= -62.0 °C<= -79.6 °F
Flash Point >= 154 °C>= 309 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
AppearanceClear, oily liquid
ColorPurple
Content<10 ppmCalcium
 <10 ppmSodium
 <30 ppmPotassium
 <50 ppmChlorine
 1185-1540 ppmSulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil Aero HF
ExxonMobil Mobil Aero HFA
ExxonMobil Exxon Hyjet V
Eastman Skydrol® 500B-4 Fire Resistant Hydraulic Fluid

PEATM5582 / 222776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.