MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient FireCon™ CPE-37-11 RoHS Black Polyethylene, Chlorinated (CPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: CPE-37-11 RoHS BLACK is a heavy duty thermoplastic jacket for power and control cables. It is suitable for VW1 and tray fire rated applications. CPE-37-11 RoHS BLACK offers the highest physical properties and flexibility, great surface quality, good heat shock resistance as well as ease of processing on large cables..

Note: Pre-drying is recommended for 4 hours at 175°-185°F. Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment. NOTE: Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 3810 sec; ASTM D2240
Tensile Strength at Break 12.4 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 350 %Type IV, 510 mm/min; ASTM D638
Tensile Modulus 6.89 MPaType IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -35.0 °CASTM D746
Oxygen Index 31 %
@Thickness 1.91 mm
ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
FormsPellets
Generic MaterialCPE
Generic NamePolyethylene, Chlorinated (CPE)
Regional AvailabilityAsia Pacific
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesCable Jacketing
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient FireCon™ CPE 30-2 Natural Chlorinated Polyethylene (CPE)
Avient FireCon™ CPE 32-33 RoHS Black Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE)
Aurora Plastics TufGuard E™ CPE 12-020 CPE, Flame Retardant
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene

PH0POL1466 / 146035

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.