MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
REXtac Rextac® RT 2330 Amorphous Polyalphaolefin (APAO)
Categories: Polymer; Thermoplastic; Polyalphaolefin; Polyolefin

Material Notes:
Adhesive and Sealant Grade.

Description: Ethylene copolymer and FDA compliant

Features: Balance of heat resistance, flexibility and stiffness, medium viscosity, and open time

Applications: Component of hot melt adhesives, sealants and specialty products

Other Properties:
Ring and Ball Softening Point (ASTM E 28): 141°C.
Needle Penetration (ASTM D 1321): 20 mm.
Shear Adhesion Failure Temperature (SAFT), Kraft/Kraft (Huntsman Method): 112°C.
Open Time, Kraft/Kraft (Huntsman Method): 20 sec.
Melt Density (190°C; Huntsman Method): 0.74 g/cc.
Flashpoint, COC (ASTM D 93): >235°C.

Information provided by Huntsman Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.860 g/ccASTM D 792
Melt Density 0.740 g/cc
@Temperature 190 °C
Huntsman Method
 0.740 g/cc
@Temperature 190 °C
Huntsman Method
Viscosity 3000 cP
@Temperature 190 °C
Melt; ASTM D-3236
 3000 cP
@Temperature 190 °C
Melt
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.820 MPaASTM D-638, D-412
 0.820 MPa
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 112 °CShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
 112 °CShear Adhesion Failure Temperature (SAFT), Kraft/Kraft; Huntsman Method
Glass Transition Temp, Tg -29.0 °CASTM D-3418
 -29.0 °C
Flash Point >= 235 °CCOC; ASTM D 93
 >= 235 °CCOC; ASTM D 93
Ring & Ball Softening Point 141 °CASTM E 28
 141 °CASTM E 28
 
Processing PropertiesOriginal ValueComments
Pot Life 20.0 secOpen Time; ASTM D-4497
 20.0 secOpen Time, Kraft/Kraft; Huntsman Method
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 Yes
 
Descriptive Properties
Needle Penetration (mm)20ASTM D 1321

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
REXtac Rextac® RT 2215 Amorphous Polyalphaolefin (APAO)
REXtac Rextac® RT 2535 Amorphous Polyalphaolefin (APAO)
Solvay Engineered Polymers SEQUEL® 2330 Engineered Polyolefin
Silon Taborex TA 2330 HD Catalyst Masterbatch
REXtac Rextac® RT 2315 Amorphous Polyalphaolefin (APAO)

PHUN06 / 47626

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.