MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Silon Taborex TA 2330 HD Catalyst Masterbatch
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TABOREX TA 1117 HD. TA 2330 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned grafted Polyethylene Compound TA 2330 HD Masterbatch completes a Sioplas System in white colour, approx. RA 9016. In addition TA 2330 HD provides processing and long term stabilisation for this system.

Information provided by Silon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.590 g/cc0.0213 lb/in³
Density 1.09 g/cc0.0394 lb/in³
Volatiles <= 0.25 %<= 0.25 %
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Storage Temperature <= 25.0 °C<= 77.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay Engineered Polymers SEQUEL® 2330 Engineered Polyolefin
REXtac Rextac® RT 2330 Amorphous Polyalphaolefin (APAO)
Evonik TEGOMER® E-Si 2330 Additive
Aremco Aremco-Bond™ 2330 High Performance Epoxide

PSILON15 / 83553

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.