Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcements, 33% Filler by Weight Additive: Lubricant, Heat Stabilizer and UV Stabilizer Features: Lubricated, Good UV Resistance and Heat Stabilized Information provided by TP Composites, Inc. |