MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.

Applications: It has good mechanical properties, it is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. It is used in the automotive industry and electrical sectors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
Water Absorption 0.92 %
@Temperature 23.0 °C,
Time 86400 sec
0.92 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 193 MPa28000 psiISO 527 Type 1A
Elongation at Break 3.1 %3.1 %ISO 527 Type 1A
Tensile Modulus 10.2 GPa1480 ksiISO 527 Type 1A
Flexural Modulus 9.66 GPa1400 ksiISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²7.14 ft-lb/in²ISO 180/1eA
Charpy Impact, Notched 1.59 J/cm²7.57 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Dielectric Constant 3.83.8IEC 60250
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 550 V550 VSolution A; IEC60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
1210
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
1200 °F
@Thickness 0.0630 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 225 - 230 °C437 - 446 °F
Front Barrel Temperature 240 - 250 °C464 - 482 °F
Mold Temperature 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone230-240°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre
E-Polymers EFLEX® V1040 EPDM/TPV
Ethylene Propylene Rubber (EPM, EPDM)
Polykemi AB POLYelast TPE E606 Thermoplastic Elastomer, EPDM-based
Techmer ES HiFill® PA6 GF HS UV 33% Glass Filled

PRHOD769 / 138000

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.