MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injection molding product range. It is processable at low temperatures and offers a specially designed, flexible material suitable for moldings.

Performance Features:

  • Excellent ambient & low temperature flexibility
  • Short cycle times
  • Phthalate free
  • Good melt flow
  • Easy demolding
  • Excellent hydrolysis & microbial resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccInjection molded; ASTM D792
Linear Mold Shrinkage 0.0080 in/inInjection molded; ASTM D955
Melt Index of Compound 50 g/10 min
@Load 10.0 kg,
Temperature 190 °C
MVR, [cm3/10 min]
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73Injection molded parts; ASTM D2240
Hardness, Shore D 23Injection molded parts; ASTM D2240
Tensile Strength at Break 30.0 MPa0.025" extruded film,; DIN 53504
Elongation at Break 820 %0.025" extruded film; DIN 53504
100% Modulus 0.00850 GPa
@Strain 100 %
0.025" extruded film; DIN 53504
300% Modulus 0.00900 GPa
@Strain 300 %
0.025" extruded film; DIN 53504
Tear Strength 257 pli0.025" extruded film; DIN 53515
Abrasion 60mm3, Injection molded; DIN 53516
Compression Set 23 %
@Temperature 22.8 °C,
Time 252000 sec
Injection molded; ASTM D395
 39 %
@Temperature 70.0 °C,
Time 86400 sec
Injection molded; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 122 - 155 °C0.025" extruded film,
 
Processing PropertiesOriginal ValueComments
Feed Temperature 185 °C
Middle Barrel Temperature 185 °C
Adapter Temperature 185 °C
Die Temperature 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Platilon® 2102 A Polyurethane (Ester) Film
Covestro Platilon® U04/PE Polyurethane (Ester) Film
Covestro Platilon® 4100 D Polyurethane (Ester) Film
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Covestro Texin® 1210 Thermoplastic Polyurethanes (TPU)

PHUQ089 / 159462

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.