MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injection molding product range. It is processable at low temperatures and offers a specially designed, flexible material suitable for moldings.

Performance Features:

  • Excellent ambient & low temperature flexibility
  • Short cycle times
  • Phthalate free
  • Good melt flow
  • Easy demolding
  • Excellent hydrolysis & microbial resistance

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³Injection molded; ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm0.0080 in/inInjection molded; ASTM D955
Melt Index of Compound 50 g/10 min
@Load 10.0 kg,
Temperature 190 °C
50 g/10 min
@Load 22.0 lb,
Temperature 374 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373Injection molded parts; ASTM D2240
Hardness, Shore D 2323Injection molded parts; ASTM D2240
Tensile Strength at Break 30.0 MPa4350 psi0.025" extruded film,; DIN 53504
Elongation at Break 820 %820 %0.025" extruded film; DIN 53504
100% Modulus 8.50 MPa
@Strain 100 %
1230 psi
@Strain 100 %
0.025" extruded film; DIN 53504
300% Modulus 9.00 MPa
@Strain 300 %
1310 psi
@Strain 300 %
0.025" extruded film; DIN 53504
Tear Strength 45.1 kN/m257 pli0.025" extruded film; DIN 53515
Abrasion 6060mm3, Injection molded; DIN 53516
Compression Set  23 %
@Temperature 22.8 °C,
Time 252000 sec
23 %
@Temperature 73.0 °F,
Time 70.0 hour
Injection molded; ASTM D395
 39 %
@Temperature 70.0 °C,
Time 86400 sec
39 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 122 - 155 °C252 - 311 °F0.025" extruded film,
 
Processing PropertiesMetricEnglishComments
Feed Temperature 185 °C365 °F
Middle Barrel Temperature 185 °C365 °F
Adapter Temperature 185 °C365 °F
Die Temperature 190 °C374 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Platilon® 2102 A Polyurethane (Ester) Film
Covestro Platilon® U04/PE Polyurethane (Ester) Film
Covestro Platilon® 4100 D Polyurethane (Ester) Film
Huntsman IROGRAN® A 85 E 4607 E TPU-Polyester
Covestro Texin® 1210 Thermoplastic Polyurethanes (TPU)

PHUQ089 / 159462

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.