MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Bio-Flex® A 4100 CL Compostable PLA Blend
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any starch or starch derivatives. Bioplastics generally replace conventional materials such as low density polyethylene (LDPE), high density polythene (HDPE) as well as polystyrene (PS) and polypropylene (PP). For packaging applications these materials need to be converted into film which is as thin as possible while maintaining high tensile strength. Depending on the specific application, packaging films have to provide a high barrier against humidity, oxygen and aromas or alternatively provide adequate permeability (“breathability”).

Information Provided by FKuR Kunststoff GmbH

Key Words: Polylactic Acid; biodegradable film
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.820 g/ccISO 60
Density 1.24 g/ccISO 1183
Water Vapor Transmission 170 g/m²/day
@Thickness 0.0200 mm
ISO 15 106-3
Oxygen Transmission Rate 130 cc/m²/day
@Thickness 0.0200 mm
1 bar; ISO 15 105-2
Nitrogen Transmission 1.646 cc-mm/m²-24hr-atm
@Thickness 0.0250 mm
DIN 53380-2
Melt Flow 10 - 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 22.0 MPaISO 527
Film Tensile Strength at Yield, MD 44.0 MPaISO 527
Film Tensile Strength at Yield, TD 42.0 MPaISO 527
Tensile Strength, Yield 44.0 MPaISO 527
Film Elongation at Break, MD 290 %ISO 527
Film Elongation at Break, TD 280 %ISO 527
Elongation at Break 12 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 904 MPaFilm, MD; ISO 527
 1120 MPaFilm, TD; ISO 527
 1840 MPaISO 527
Flexural Strength 48.0 MPaat 3.5% strain; ISO 178
Flexural Modulus 1770 MPaISO 178
Charpy Impact Unnotched 44.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
Elmendorf Tear Strength, MD 1.12 g/milASTM D 1922
Elmendorf Tear Strength, TD 0.918 g/milASTM D 1922
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 155 °CISO 3146-C
Vicat Softening Point 44.0 °CA; ISO 306
Heat Distortion Temperature 40.0 °CHDT B; ISO 75
 
Descriptive Properties
Melt Volume Flow (cm3/10 min)9-11ISO 1133; 190°C, 2.16kg
Spencer Impact Test (N/mm)14ASTM D 3420

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polylactic Acid (PLA) Biopolymer
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend
BASF Ecovio® C2224 F Blend Biodegradable Polyester
BASF Ecovio® C2332 F Blend Biodegradable Polyester

PFKUR001 / 107039

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.