MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Polyester Glass and Mineral Filled BMC
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass and Mineral Filled BMC

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyester Glass and Mineral Filled BMC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 - 2.27 g/ccAverage value: 1.89 g/cc Grade Count:49
Water Absorption 0.0500 - 0.500 %Average value: 0.132 % Grade Count:47
Linear Mold Shrinkage 0.000 - 0.0150 cm/cmAverage value: 0.00265 cm/cm Grade Count:47
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 10.0 - 70.0Average value: 42.2 Grade Count:39
Hardness, Rockwell E 51.0 - 78.0Average value: 62.3 Grade Count:8
Tensile Strength, Ultimate 12.0 - 117 MPaAverage value: 54.0 MPa Grade Count:49
Elongation at Break 0.590 - 1.32 %Average value: 0.929 % Grade Count:8
Modulus of Elasticity 6.00 - 20.2 GPaAverage value: 12.6 GPa Grade Count:13
Flexural Yield Strength 30.0 - 248 MPaAverage value: 126 MPa Grade Count:49
Flexural Modulus 6.00 - 18.3 GPaAverage value: 11.9 GPa Grade Count:21
Compressive Yield Strength 75.8 - 228 MPaAverage value: 159 MPa Grade Count:47
Poissons Ratio 0.290 - 0.390Average value: 0.323 Grade Count:9
Shear Modulus 2.30 - 7.77 GPaAverage value: 5.11 GPa Grade Count:7
Izod Impact, Notched 0.330 - 15.5 J/cmAverage value: 3.14 J/cm Grade Count:45
Charpy Impact, Notched 0.271 - 0.900 J/cm²Average value: 0.469 J/cm² Grade Count:9
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.91e+14 - 3.10e+15 ohm-cmAverage value: 1.56e+15 ohm-cm Grade Count:9
Dielectric Constant 4.20 - 6.10Average value: 4.99 Grade Count:20
Dielectric Strength 11.1 - 16.9 kV/mmAverage value: 13.7 kV/mm Grade Count:40
Dielectric Breakdown 22900 - 23000 VAverage value: 23000 V Grade Count:7
 23000 - 23000 V
@Temperature 121 - 121 °C
Average value: 23000 V Grade Count:1
 23000 - 23000 V
@Time 3600 - 3600 sec
Average value: 23000 V Grade Count:1
Dissipation Factor 0.00700 - 0.0201Average value: 0.0154 Grade Count:20
Arc Resistance 170 - 210 secAverage value: 187 sec Grade Count:41
Track Resistance 5400 - 60000 secAverage value: 31200 sec Grade Count:4
Comparative Tracking Index 500 - 600 VAverage value: 571 V Grade Count:38
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 - 54.0 µm/m-°CAverage value: 36.0 µm/m-°C Grade Count:4
 43.0 - 86.0 µm/m-°C
@Temperature 40.0 - 130 °C
Average value: 62.6 µm/m-°C Grade Count:5
Thermal Conductivity 0.720 - 0.910 W/m-K
@Temperature 100 - 100 °C
Average value: 0.833 W/m-K Grade Count:3
Maximum Service Temperature, Air 170 - 223 °CAverage value: 208 °C Grade Count:9
Deflection Temperature at 1.8 MPa (264 psi) 127 - 316 °CAverage value: 253 °C Grade Count:49
Glass Transition Temp, Tg 155 - 170 °CAverage value: 164 °C Grade Count:4
Flammability, UL94 HB - 5VBGrade Count:48
Oxygen Index 25.0 - 47.0 %Average value: 36.6 % Grade Count:7
 
Processing PropertiesOriginal ValueComments
Processing Temperature 140 - 171 °CAverage value: 151 °C Grade Count:3
Mold Temperature 138 - 182 °CAverage value: 152 °C Grade Count:38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
A. Schulman BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 695 Vinyl Ester Molding Compound
Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled
Overview of materials for Thermoset Polyester Glass SMC

O3511 / 78220

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.