Notes: Sarlink EE-2340DN XRD is a general purpose thermoplastic elastomer used in automotive applications. Sarlink EE-2340DN XRD is a high hardness grade with good UV resistance. This grade can be processed by extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: High Density; High Hardness; Low Temperature Toughness; Ozone Resistant; Sunlight Resistant; UV Resistant; Weather Resistant Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |