MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Monprene® CP-3090D XRD Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene CP-3090D XRD, available in NAT, is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-3090D XRD is a low density, high hardness, filled grade that is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Filled; Low Flow; High Hardness; Low Density; Low Specific Gravity

Uses: Consumer Applications; General Purpose; Profiles

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  40
@Time 5.00 sec
40
@Time 0.00139 hour
Injection Molded; ASTM D2240
 42
@Time 1.00 sec
42
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 12.5 MPa1810 psi20 in/min, Across Flow; ASTM D412
 13.0 MPa1890 psi20 in/min, Flow; ASTM D412
Tensile Stress at Strain  8.83 MPa
@Strain 100 %
1280 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 9.17 MPa
@Strain 300 %
1330 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 12.6 MPa
@Strain 100 %
1830 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 13.0 MPa
@Strain 300 %
1890 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 310 %310 %20 in/min, Flow; ASTM D412
 700 %700 %20 in/min, Across Flow; ASTM D412
Tear Strength 71.0 kN/m405 pli20 in/min, Across Flow; ASTM D624
 104 kN/m594 pli20 in/min, Flow; ASTM D624
Compression Set 77 %
@Temperature 70.0 °C
77 %
@Temperature 158 °F
Type 1; ASTM D395B
 49 %
@Temperature 22.8 °C,
Time 79200 sec
49 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 227 °C390 - 440 °FMelt, Injection
Rear Barrel Temperature 182 - 204 °C360 - 400 °FInjection
Middle Barrel Temperature 188 - 210 °C370 - 410 °FInjection
Front Barrel Temperature 199 - 216 °C390 - 420 °FInjection
Nozzle Temperature 199 - 227 °C390 - 440 °FInjection
Zone 1 182 - 216 °C360 - 420 °FExtrusion
Zone 2 182 - 216 °C360 - 420 °FExtrusion
Zone 3 182 - 216 °C360 - 420 °FExtrusion
Zone 4 182 - 216 °C360 - 420 °FExtrusion
Zone 5 182 - 216 °C360 - 420 °FExtrusion
Die Temperature 182 - 216 °C360 - 420 °FExtrusion
Mold Temperature 15.6 - 43.3 °C60.0 - 110 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 25A, Non-Black Sulfur Cure
Wacker ELASTOSIL® R plus 4105/40 Solid Silicone Rubber-Batch Grade
Wacker Elastosil® R plus 4001/30 Silicone Rubber
Teknor Apex Sarlink® TPE EE-2340DN XRD Thermoplastic Elastomer
NuSil VersaSil 40 MED-4042 Silicone

PTEKNQ0849 / 237340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.