MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Superwool® VF Shapes and Boards Plus Carton Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool® Plus™ Carton is produced by the addition of selected Superwool ®Plus™ fibers, both organics and inorganics binders. Boards in Superwool®Plus Carton are thin and rigid.

Typical applications:

  • Riser sleeves and crucibles for ferrous and non ferrous molten metals
  • Stopper nut insulation
  • Ladle shroud gasket
  • Nozzle insulation in continuous casting
  • Roller inserts in roller hearth furnace
  • Glass casting mould
  • Tube insulation end in tube fumes boiler
  • Insulation for domestic appliance
  • Furnace insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.290 g/cc0.0105 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00147 GPa0.213 ksiunfired
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 400 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 752 °F
ASTM C-201
 0.100 W/m-K
@Temperature 600 °C
0.694 BTU-in/hr-ft²-°F
@Temperature 1110 °F
ASTM C-201
 0.150 W/m-K
@Temperature 800 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1470 °F
ASTM C-201
Shrinkage <= 2.0 %
@Temperature 1100 °C,
Time 86400 sec
<= 2.0 %
@Temperature 2010 °F,
Time 24.0 hour
isothermal, permanent
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 7.0 %7.0 %
 
Descriptive Properties
Classification Temperature (°C)1200
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin
Overview of materials for AISI 4000 Series Steel
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Overview of materials for AISI 1000 Series Steel

CMORF7018 / 203317

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.