Visico™ LE4421M / Visico™ LE4431M is a two-part silane crosslinkable insulation system, specially designed for insulation applications. Applications: Visico™ LE4421M / Visico™ LE4431M is intended for insulation of XLPE medium voltage cables with rated voltages up to 36 kV. Specifications: Visico™ LE4421M / Visico™ LE4431M in combination meets these applicable requirements when processed using sound extrusion and testing procedure: ASTM D 1248 Type I, Class A, Category 4; IEC 60502; HD 603 S1; HD 604 S1; and HD 620 S1.Information provided by Borealis AG |