MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

China Tungsten YG9X Tungsten Carbide Powder
Categories: Ceramic; Carbide

Material Notes:

Information provided by China Tungsten

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.20 g/cc0.116 lb/in³Scott
Density 14.6 g/cc0.527 lb/in³
Binder 2.02.0wax
Particle Size 0.80 µm0.80 µm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A 9292
Tensile Strength, Ultimate 2000 MPa290000 psi
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 9.0 %9.0 %
Other 0.20 %0.20 %
WC 90.8 %90.8 %
 
Descriptive Properties
Flow Rate; sec/50g30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 3 PM cast
Sandvik H10F Cemented Carbide for Can Tooling
Kennametal Stellite Stellite® 3 PM with P/M Processing
NAECO® NAECOMET® 1000 AMS-T-21014 AMS-7725 ASTM B777 High Density Machinable Tungsten
H.C. Starck Amperit® 519.074 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)

NCHIN012 / 78854

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.