MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Styrolux® BX6400 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux BX6400 is a developmental styrene butadiene copolymer (SBC) of high clarity and ultimate toughness used mainly in sheet and film extrusion and thermoforming applications. It is specifically designed for improved performance in blends with general-purpose polystyrene, providing parts with an excellent balance of toughness and transparency.
  • Outstanding toughness
  • High GPPS blend capability
  • Excellent clarity

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
ISO 62
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 97ISO 868
Hardness, Shore D 58ISO 868
Tensile Strength, Yield 15.0 MPaISO 527
Elongation at Break 300 %ISO 527
Elongation at Yield 2.0 %ISO 527
Tensile Modulus 900 MPaISO 527
Flexural Strength 18.0 MPaISO 178
Flexural Modulus 900 MPaISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 NB
@Temperature 23.0 °C
ASTM D 256
 NB
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179
 NB
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 85.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 35.0 °C
@Load 1.02 kg
50°C/h; ISO 306
 67.0 °C
@Load 5.10 kg
50°C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D 1003
Transmission, Visible >= 89 %
@Wavelength 550 nm
ASTM D 1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 230 °CISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
Chi Mei Kibiton® PB-5903 SBC
INEOS Styrolution Styrolux® S SBC
Overview of materials for Styrene-Butadiene Copolymer, SBC
BASF Styroclear GH 62 SBC

PBASF8026 / 159708

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.