Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by Weight Additive: Heat Stabilizer and Lubricant Features: Heat Stabilized and Lubricated Appearance: Black TPCI# 7151102 Information provided by TP Composites, Inc. |