MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for automotive engine covers, housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.1 - 2.5 %2.1 - 2.5 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 6.9 - 7.5 %6.9 - 7.5 %ISO 62
Viscosity Measurement 123123ISO 307
Melt Flow 116.45 g/10 min
@Load 5.00 kg,
Temperature 275 °C
116.45 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 115 MPa16700 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 3.60 GPa522 ksiISO 527-1/-2
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 6.2
@Frequency 1e+6 Hz
6.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.20
@Frequency 1e+6 Hz
0.20
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.30 J/g-°C0.311 BTU/lb-°F
Melting Point 220 °C428 °FDIN 53765
Maximum Service Temperature, Air 180 °C356 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 290 °C482 - 554 °FInjection-molding/Extrusion
Mold Temperature 70.0 - 90.0 °C158 - 194 °FInjection-molding
 
Descriptive Properties
ColorBK 23210
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry)
BASF Ultramid® B3WGM24 BK30564 10/20% Glass/Mineral Filled PA6 (Conditioned)
BASF Ultramid® 8266G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
BASF Ultramid® 8260 HS PA6 (Dry)
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled

PBASG0277 / 131910

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.