MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sinvicomp SRF 1807 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Availability: Asia Pacific

Features: Good Flow; Good Impact Resistance

Uses: Fittings

Forms: Pellets

Processing Method: Injection Molding

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70ASTM D2240
Tensile Strength, Yield 7050 psi9.8 in/min; ASTM D638
Elongation at Break 100 %9.8 in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 374 °F
@Time >=3600 sec
Congo Red; BS 2782
Vicat Softening Point 138 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy
Karina 18/387-RG-GE (CS) Gray Color Concentrate for PVC
Addiplast Addilene J 470 ST14 Polypropylene Copolymer
A.D. Compound Adene NCTAG Copolymer 50% CaCO3 Filled Polypropylene

PTEKNO994 / 129175

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.