MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® EP950NMF Gray Non-Metallic Filled Rubber Modified Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP950NMF Gray is a non-metallic filled version of EP950G. It is a one-part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It has a medium paste like viscosity, which gives minimal sag upon cure at elevated temperature. Being a 100% solids, single component product a variety of simple, low cost dispensing methods are available for application of this product. This product will cure at temperatures as low as 113°C (235°F) without sacrificing shelf life or need for unusual shipping or storage considerations.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccTM R050-16
Water Absorption 2.08 %
@Time 86400 sec
2.08 %
@Time 24.0 hour
TM R050-35
Viscosity 750000 cP750000 cPRVT, #7, 2.5 rpm; TM R050-12
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565TM R050-17
Tensile Strength at Break 37.9 MPa5500 psiTM R050-36
Tensile Strength, Ultimate 37.9 MPa5500 psiTM R050-36
Tensile Strength, Yield 17.2 MPa2500 psiTM R050-36
Elongation at Break 1.0 - 2.0 %1.0 - 2.0 %TM R050-36
Tensile Modulus 4.14 GPa600 ksiTM R050-36
Adhesive Bond Strength 17.2 MPa2500 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Peel Strength 0.877 - 1.23 kN/m5.00 - 7.00 pli
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8.00e+12 ohm-cm8.00e+12 ohm-cm
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
4.5
@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 16.1 kV/mm410 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 130 µm/m-°C72.2 µin/in-°F
Thermal Conductivity 0.210 W/m-K1.46 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C347 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 123 °C253 °FTM R050-25
 
Processing PropertiesMetricEnglishComments
Cure Time  20.0 min
@Temperature 177 °C
0.333 hour
@Temperature 351 °F
 40.0 min
@Temperature 150 °C
0.667 hour
@Temperature 302 °F
 45.0 min
@Temperature 135 °C
0.750 hour
@Temperature 275 °F
 150 min
@Temperature 121 °C
2.50 hour
@Temperature 250 °F
Pot Life  130000 min
@Temperature 25.0 °C
130000 min
@Temperature 77.0 °F
Mass: 100g
 259000 min
@Temperature <=10.0 °C
259000 min
@Temperature <=50.0 °F
Mass: 100g
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Sinvicomp SRF 1807 Polyvinyl Chloride, Rigid
Karina 18/387-RG-GE (CS) Gray Color Concentrate for PVC
Addiplast Addilene J 470 ST14 Polypropylene Copolymer

PRESL153 / 101567

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.