MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Baydur® 683 Polyurethane Structural Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Characterization: Baydur 683 is a rigid polyurethane structural foam system that is formulated for “hand cast ” operations.

Properties / Applications: Baydur 683 is a rigid polyurethane structural foam system that is formulated for “hand cast ” operations. It has a long open time to allow for adequate mixing and pouring without use of RIM machinery. The system can still be utilized with RIM equipment, however reactivity times are shortened accordingly. The system is supplied as two reactive components. Component A is a polymeric diphenylmethane diisocyanate (PMDI), and Component B is a formulated polyol system containing no CFC- or HCFC-blowing additives. The Baydur 683 system is used for applications requiring high compression strength foams,filling cavities and/or producing foam cores for overmolding. As with any product, use of the Baydur 683 system in a given application must be tested (including field testing, etc.) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.0641 g/cc
 1.08 g/ccPolyol (Component B)
 1.25 g/ccIsocyanate (Component A)
Viscosity 200 cPIsocyanate (Component A)
 900 cPPolyol (Component B)
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.538 MPa
Compressive Modulus 2535 psi
 
Processing PropertiesOriginal ValueComments
Gel Time <= 2.50 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Avient OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, PUR
Covestro Baydur® 645 Polyurethane Structural Foam RIM, Density 15 pcf
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam

PCOVEST0086 / 201869

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.