MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

LFT compounds can be processed using equipment similar to that used for short fiber products. The mechanical properties of finished parts depend greatly on the length of the fibers in the molded part; therefore processing conditions must be set carefully in order to minimize fiber breakage. A low shear process is advised, with low back pressure, low screw speed and low-to-medium injection speed. This grade must be dried in a desiccant dryer with a dew point set at -40°C.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.60 g/cc1.60 g/ccASTM D792
Filler Content 50 %50 %Long Glass Fiber
Linear Mold Shrinkage, Flow 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 241 MPa35000 psiASTM D638
Elongation at Break 2.0 - 3.0 %2.0 - 3.0 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 14.5 GPa2100 ksiType I, 5.1 mm/min; ASTM D638
Flexural Yield Strength 352 MPa51100 psiASTM D790
Flexural Modulus 15.2 GPa2200 ksiASTM D790
Izod Impact, Notched 4.50 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
8.43 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
Izod Impact, Unnotched 16.0 J/cm30.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 114 °C237 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 80.0 °C176 °F
Drying Temperature 90.0 °C194 °F
Dry Time 8.00 - 12.0 hour8.00 - 12.0 hour
 
Descriptive Properties
FormsPellets
Generic MaterialPUR, Unspecified
Generic NamePolyurethane, Unspecified (PUR, Unspecified)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66)
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced

PH0POL1076 / 145645

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.