MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Visico™/Ambicat™ LE4427/LE4476 Polyethylene Compound, Crosslinkable  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Visico™ LE4427 / Ambicat™ LE4476 is a silane crosslinkable black compound designed for weather resistant covering/insulation of overhead and façade cables. The black base material Visico™ LE4427 in combination with the catalyst masterbatch Ambicat™ LE4476 will accelerate the moisture-induced crosslinking reaction. The system is highly active and crosslinks quickly at ambient conditions, in sauna or in hot water. When properly mixed, addition of 5 parts of Ambicat™ LE4476 to 95 parts of Visico™ LE4427 , insulation with excellent thermo-oxidative stability, also in contact with copper as well as aluminum, is achieved. Applications: Weather resistant covering/insulation of overhead and façade cables. Additives: Visico™ LE4427 / Ambicat™ LE4476 contains antioxidant, metal deactivator and a drying agent. Visico™ LE4427 contains a permanent scorch retardant additive, ensuring safe processing and enabling the use of a highly active crosslinking catalyst. Specifications: ANSI/ICEA S-70-547; ASTM D 1248 Type II, Class C, Category 4; HD 603 S1; HD 626 S1 (TIX-1, TIX-3, TIX-5, TIX-7, TIX8); NF C33-209 part 6-2 (Except messenger wire); NEMA WC 70; and NEMA WC 71.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³mixture 95:5; ISO 1183/ISO 1872-2
ESCR 10% Igepal® >= 96 hour
@Temperature 50.0 °C
>= 96 hour
@Temperature 122 °F
F20; IEC 60811-4-1/B
Carbon Black Loading 2.5 %2.5 %ISO 6964
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 10.5 MPa<= 1520 psiafter aging (6 weeks); IEC 60811-1-2
 <= 11.25 MPa<= 1632 psiafter aging (240h, 135°C); IEC 60811-1-2
 <= 12.75 MPa<= 1849 psiafter aging (3-6 weeks); IEC 60811-1-2
 >= 15.0 MPa>= 2180 psi250mm/min; ISO 527
Elongation at Break >= 300 %>= 300 %250mm/min; ISO 527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1e+05>= 1e+05IEC 60093
Dielectric Constant 2.9
@Frequency 50000 Hz
2.9
@Frequency 50000 Hz
IEC 60250
Dissipation Factor 0.0010
@Frequency 50000 Hz
0.0010
@Frequency 50000 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -76.0 °C<= -105 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Zone 1 150 °C302 °F
Zone 2 170 °C338 °F
Zone 3 170 °C338 °F
Zone 4 170 °C338 °F
Die Temperature 170 °C338 °F
Shelf Life 15.0 Month15.0 Month
 
Descriptive Properties
Hot Set Test, %30200°C, 0.3 MPa;IEC 60811-2-1; Elongation under load

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Polidan® T/A Polyethylene, Crosslinked (XLPE)
Borealis LE4201R Polyethylene Insulation Compound, Crosslinkable
Avient Syncure™ System S112NA Polyethylene, Crosslinked (XLPE)
Borealis Borlink™ LE4244EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable

PBOREA605 / 108864

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.