MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
W-25 Re Tungsten Rhenium Alloy, Deformed
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Deformed applies only to tensile; other property values are typical of this alloy. Ductile to brittle transition temperature (DBBT) (-100) - (25) °C. Stress relieving temperature 1200-1400°C. Recrystallization Temperature 1500-1650°C. Bcc crystal lattice.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 19.7 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 2750 - 4900 MPaVacuum-melted
Elongation at Break 1.5 %
Modulus of Elasticity 430 GPa
Poissons Ratio 0.29
Shear Modulus 159 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000290 ohm-cmTemp Coefficient is 0.00115/°C 20-1000°C.
Critical Superconducting Temperature 4.20 K
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.48 µm/m-°C
@Temperature 500 °C
 5.04 µm/m-°C
@Temperature 1000 °C
Specific Heat Capacity 0.140 J/g-°C
 0.156 J/g-°C
@Temperature 1000 °C
Melting Point 3050 °C
 
Component Elements PropertiesOriginal ValueComments
Rhenium, Re 25 %
Tungsten, W 75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
W-25 Re Tungsten Rhenium Alloy, Annealed
Goodfellow Tungsten 75/Rhenium 25 Alloy
Park Aerospace Nelcote® F-502 Phenolic Prepreg, Silica Reinforced
Park Aerospace Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
W-3 Re Tungsten Rhenium Alloy

MWRe05 / 14309

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.