MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Park Aerospace Nelcote® F-502 Phenolic Prepreg, Silica Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rocket nozzles, as well as ducting and secondary structures. GMS4001 qualified specifications.

Key Features and Benefits:

  • Provides a combination of high-strength and ablative properties for demanding applications
  • Low thermal expansion
  • Good Tack and Drape properties
  • Conforms to MIL-R-9299 Type B

Applications/Qualifications:

  • Rocket Nozzles
  • Ducting
  • Secondary Structures

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 g/cc1.70 g/ccASTM D792
Volatiles 6.0 - 10 %
@Temperature 135 °C
6.0 - 10 %
@Temperature 275 °F
8 min
Thickness 711 microns28.0 milcured laminate, per ply
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 7070ASTM D2583
Tensile Strength, Yield 89.6 MPa
@Temperature 23.9 °C
13000 psi
@Temperature 75.0 °F
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638
Tensile Modulus 16.5 GPa
@Temperature 23.9 °C
2400 ksi
@Temperature 75.0 °F
0° Direction, Dry; 325°F, 1000psi Cured; ASTM D638
Flexural Strength 159 MPa
@Temperature 23.9 °C
23000 psi
@Temperature 75.0 °F
Dry; 325°F, 1000psi Cured; ASTM D790
Flexural Modulus 17.2 GPa
@Temperature 23.9 °C
2500 ksi
@Temperature 75.0 °F
Dry; 325°F, 1000psi Cured; ASTM D790
Compressive Strength 165 MPa
@Temperature 23.9 °C
24000 psi
@Temperature 75.0 °F
Dry; 325°F, 1000psi Cured; ASTM D695
Compressive Modulus 16.5 GPa
@Temperature 23.9 °C
2400 ksi
@Temperature 75.0 °F
Dry; 325°F, 1000psi Cured; ASTM D695
 
Processing PropertiesMetricEnglishComments
Gel Time 0.800 - 1.70 min0.800 - 1.70 min
Shelf Life  3.00 Month
@Temperature 4.44 °C
3.00 Month
@Temperature 40.0 °F
 6.00 Month
@Temperature -17.8 °C
6.00 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)610
Prepreg Resin Content (%)31-37
Resin Flow (%)10-30325°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Park Aerospace Nelcote® F-554 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Park Aerospace Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Park Aerospace Nelcote® F-557 Phenolic Prepreg, Commercial Silica Fabric Reinforced
Park Aerospace Nelcote® F-557 Phenolic Prepreg, Aerospace Silica Fabric Reinforced
Overview of materials for Phenolic, Carbon Fiber Composite

PPARK048 / 89320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.