MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
FKuR Kunststoff Biograde® C 5509 CL Cellulose Acetate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: Biograde® C 5509 CL is a transparent cellulose based compound, which is used in injection molding applications. It contains a high proportion of renewable raw materials and has a biobased carbon content (,Biobased Carbon Content ') of more than 60%. Biograde® C 5509 CL can be processed on standard injection molding machines with universal screws easily, even on tools with multiple cavities. This compound can be dyed easily and is suitable for food contact. Partly biobased polymer compound suitable for transparent injection molding applications. The biobased carbon content (BCC) is > 60 % (calculated).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Melt Flow 40 - 56 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 48.0 MPaISO 527
Tensile Strength, Ultimate 48.0 MPaISO 527
Tensile Strength, Yield 48.0 MPaISO 527
Elongation at Break 15.5 %ISO 527
Modulus of Elasticity 2.32 GPaISO 527
Tensile Modulus 2320 MPaISO 527
Charpy Impact Unnotched 165 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 180 °CISO 3146-C
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °CHDT B; ISO 75
Vicat Softening Point 100 °CISO 306
 
Descriptive Properties
Bio-based carbon content (%)60ASTM D 6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
Lucobit Lucocell® FG3000 Cellulose Asphalt Additive
Rotuba H Cellulose Acetate
Rotuba 855, Slow Burning Ethyl Cellulose
Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate

PFKUR911 / 192731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.