MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rotuba H Cellulose Acetate
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Cellulosic; Cellulose Acetate, Molded

Material Notes: Property values at 50% RH.

Data provided by the manufacturer.

Key Words: Rotuba Plastics; Cellulosic; CA
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Water Absorption 2.3 %2.3 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7676ASTM D785
Tensile Strength, Ultimate 40.0 MPa5800 psiASTM D638
Tensile Strength, Yield 30.0 MPa4350 psiASTM D638
Elongation at Break 39 %39 %ASTM D638
Flexural Yield Strength 46.0 MPa6670 psiASTM D790
Flexural Modulus 0.120 GPa17.4 ksiASTM D790
Izod Impact, Notched 2.08 J/cm3.90 ft-lb/inASTM D256
 0.590 J/cm
@Temperature -40.0 °C
1.11 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 155 °C311 °FFlow temperature, ASTM D569
 
Processing PropertiesMetricEnglishComments
Processing Temperature 210 °C410 °FCenter barrel temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate
FKuR Kunststoff Biograde® C 5509 CL Cellulose Acetate
Lucobit Lucocell® FG3000 Cellulose Asphalt Additive
Rotuba 855, Slow Burning Ethyl Cellulose
Hybrid Plastics Nanoreinforced® Cellulose Propionate Acetate

PECR04 / 35480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.