MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® FE310001 NC010 Nylon 612  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Zytel® FE310001 NC010 is a high viscosity polyamide 612 resin that is suitable for extrusion applications, such as monofilaments and tubing.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.013 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPa
@Temperature 23.0 °C
DAM; ISO 527
Tensile Modulus 2250 MPa
@Temperature 23.0 °C
DAM; ISO 527
Flexural Modulus 2000 MPa
@Temperature 23.0 °C
DAM; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CDAM; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CDAM; ISO 75-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 230 - 240 °CDAM; Extrusion
 235 °CDAM; Optimum; Extrusion
 250 °CDAM; Optimum; Injection Molding
 230 - 290 °CDAM; Injection Molding
Mold Temperature 50.0 - 90.0 °CDAM; Injection Molding
 80.0 °CDAM; optimum; Injection Molding
Drying Temperature 80.0 °CDAM; Extrusion
 80.0 °CDAM; Injection Molding
Dry Time 2.00 - 4.00 hourDAM; Injection Molding
 4.00 - 6.00 hourDAM; Extrusion
Moisture Content <= 0.050 %DAM; Extrusion
 <= 0.050 %DAM; Injection Molding
 
Descriptive Properties
AppearanceNatural ColorDAM
FormsPelletsDAM
GenericNylon 612DAM
Material StatusPreliminary DataDAM
Part Marking Code>PA612<ISO 11469; DAM
Processing MethodExtrusionDAM
Product CategoryExtrusion ResinsDAM
Region Available - GlobalYesDAM
Resin IdentificationPA612ISO 1043; DAM

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 151L NC010 PA612
Celanese Zytel® 153HSL NC010 PA612
Celanese Elvamide® 8061 PA6/66/610
Celanese Zytel® 151 NC010 PA612
Celanese Zytel® 77G33HS1L NC010 Nylon 612

PZDSZ1387 / 140204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.