MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® 151 NC010 PA612
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes: Unreinforced Polyamide 612

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³DAM; ISO 1183
Melt Density 0.900 g/cc0.0325 lb/in³
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
Immersion; DAM; Sim. to ISO 62
 3.0 %
@Thickness 2.00 mm
3.0 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.30 %
@Thickness 2.00 mm
1.30 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Measurement 0.980.98Intrinsic viscosity; ISO 307, 1157, 1628
Viscosity Number 95 cm³/g0.95 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inDAM; ISO 294-4, 2577
 0.011 cm/cm
@Thickness 3.17 mm
0.011 in/in
@Thickness 0.125 in
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
 0.011 cm/cm
@Thickness 3.17 mm
0.011 in/in
@Thickness 0.125 in
Melt Flow 35 g/10 min
@Load 1.00 kg,
Temperature 230 °C
35 g/10 min
@Load 2.20 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 10810850% RH; ISO 2039-2
 114114DAM; ISO 2039-2
Tensile Strength, Yield 54.0 MPa7830 psi50% RH; ISO 527-1/-2
 62.0 MPa8990 psiDAM; ISO 527-1/-2
Elongation at Break 17 %17 %Nominal; DAM; ISO 527-1/-2
 >= 50 %>= 50 %Nominal; 50% RH; ISO 527-1/-2
Elongation at Yield 4.5 %4.5 %DAM; ISO 527-1/-2
 18 %18 %50% RH; ISO 527-1/-2
Tensile Modulus 1.70 GPa247 ksi50% RH; ISO 527-1/-2
 2.40 GPa348 ksiDAM; ISO 527-1/-2
Flexural Modulus 1.44 GPa209 ksi50% RH; ISO 178
 2.10 GPa305 ksiDAM; ISO 178
Poissons Ratio 0.380.38DAM
 0.420.4250% RH
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 4.00 kJ/m²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 4.50 kJ/m²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
 4.50 kJ/m²
@Temperature -30.0 °C
2.14 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.350 J/cm²
@Temperature -30.0 °C
1.67 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.350 J/cm²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Dielectric Strength 30.0 kV/mm762 kV/in50% RH; IEC 60243-1
 30.0 kV/mm762 kV/inDAM; IEC 60243-1
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FDAM; ISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 160 µm/m-°C
@Temperature 55.0 - 160 °C
88.9 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FDAM; ISO 11359-1/-2
 90.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
 180 µm/m-°C
@Temperature 55.0 - 160 °C
100 µin/in-°F
@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
Specific Heat Capacity 2.75 J/g-°C0.657 BTU/lb-°FMelt
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°FMelt
Melting Point 218 °C424 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FDAM; ISO 75-1/-2
Vicat Softening Point 181 °C358 °F50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 50.0 °C122 °F10°C/min; 50% RH; ISO 11357-1/-2
 65.0 °C149 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  V-2
@Thickness 0.850 mm
V-2
@Thickness 0.0335 in
DAM; IEC 60695-11-10
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Oxygen Index 27 %27 %DAM; ISO 4589-1/-2
Glow Wire Test  700 °C
@Thickness 0.750 mm
1290 °F
@Thickness 0.0295 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 1.50 mm
1290 °F
@Thickness 0.0591 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
No Flame; DAM; IEC 60335-1
 700 °C
@Thickness 3.00 mm
1290 °F
@Thickness 0.118 in
No Flame; DAM; IEC 60335-1
Glow Wire Ignition Temperature  725 °C
@Thickness 0.400 mm
1340 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-12
 725 °C
@Thickness 0.750 mm
1340 °F
@Thickness 0.0295 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 1.00 mm
1340 °F
@Thickness 0.0394 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 1.50 mm
1340 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
DAM; IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
1340 °F
@Thickness 0.118 in
DAM; IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.400 mm
1760 °F
@Thickness 0.0157 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
DAM; IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
DAM; IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 °C464 °FOptimum, Extrusion
 235 - 250 °C455 - 482 °FRange, Extrusion
 230 - 290 °C446 - 554 °FRange, Injection
Mold Temperature 50.0 - 90.0 °C122 - 194 °FInjection
Drying Temperature 75.0 - 80.0 °C167 - 176 °FExtrusion
 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 3.00 - 4.00 hour3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.15 %<= 0.15 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)7.5E-08
Emission of organic compounds (µgC/g)3.9VDA 277
FMVSS ClassDNIISO 3795 (FMVSS 302)
ISO designationISO 16396-PA612,,M1G1N,S10-020
Part Marking Code>PA612<ISO 11469
PolymerPA612
Resin IdentificationPA612ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® 151L NC010 PA612
Celanese Zytel® 158 NC010 PA612
Celanese Zytel® 101 NC010 PA66
Celanese Zytel® 153HSL NC010 PA612
Celanese Zytel® 77G33L BK031 PA612-GF33

PDSX5307 / 197947

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.