MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: Visico LE4421/LE4460/LE4437 is a natural, halogen-based, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of the Visico LE4421 base resin, along with the LE4460 brominated flame retardant masterbatch and the LE4437 tin catalyst masterbatch provides a highly scorch retardant compound with excellent thermal stability and good flame properties. LE4421/LE4460/LE4437 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder head or die.

LE4421/LE4460/LE4437 is recommended for use as insulation for low voltage control cables and power cables up to 6 kV in rating.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccLE 4421; ASTM D792
 0.941 g/ccLE 4437; ASTM D792
 2.00 g/ccLE 4460; ASTM D792
Melt Flow 0.90 g/10 minLE 4421; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 2115 psiHeat Aging (7 days at 121°C); ASTM D412
 2350 psiASTM D412
Elongation at Break <= 50 %Hot Creep Test (150°C, .2 MPa); ICEA T-28-562
 270 %Heat Aging (7 days at 121°C); ASTM D412
 300 %ASTM D412
Tensile Set <= 5.0 %Hot Creep Test (150°C,.2 MPa); ICE T-28-562
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.3
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 550 V/milASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
ASTM D150
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature >= 171 °C
Front Barrel Temperature >= 146 °C
Die Temperature >= 350 °F
Head Temperature >= 177 °C
 
Descriptive Properties
Horizontal Flame TestPass14AWG-30mil, UL 1581

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SABIC HP4023W Low Density Polyethylene for Blown Film

PBOREA197 / 27504

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.