MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC HP4023W Low Density Polyethylene for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with good mechanical properties.

Typical Applications: HP4023W can be used for high clarity laundry bags, textile wrapping films, produce bags and zip lock bags.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D1505
Thickness 30.0 microns1.18 mil
Melt Flow 4.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
4.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 7.00 MPa1020 psiASTM D882
Film Tensile Strength at Yield, TD 7.00 MPa1020 psiASTM D882
Film Elongation at Break, MD 270 %270 %ASTM D882
Film Elongation at Break, TD 540 %540 %ASTM D882
Elmendorf Tear Strength MD 150 g150 gASTM D1922
Elmendorf Tear Strength TD 120 g120 gASTM D1922
Elmendorf Tear Strength, MD 5.00 g/micron127 g/milASTM D1922
Elmendorf Tear Strength, TD 4.00 g/micron102 g/milASTM D1922
Dart Drop 2.00 g/micron50.8 g/milASTM D1709
Dart Drop Test 60.0 g0.132 lbASTM D1709
Film Tensile Strength at Break, MD 18.0 MPa2610 psiASTM D882
Film Tensile Strength at Break, TD 15.0 MPa2180 psiASTM D882
1% Secant Modulus, MD 60.0 MPa8700 psiASTM D882
1% Secant Modulus, TD 170 MPa24700 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 91.0 °C196 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003
Gloss 75 %75 %at 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 175 °C320 - 347 °F
Blow-up Ratio (BUR) 2.0 - 3.02.0 - 3.0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Visico™ LE4421/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
SABIC HP0722N Low Density Polyethylene for Blown Film
SABIC F00952EQ High Density Polyethylene for Blown Film
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer

PSABICZ824 / 133020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.