MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Murylon® 6 Cast Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: Murylon® 6 CAST has extremely low levels of residual stress thanks to the casting procedure used to produce it. This material is therefore ideally suited to extensively processed components.

Special Properties:
• Good impact resistance
• Low cold flow characteristics
• Optimized wear properties
• Low residual stress
• Flexible production of large-volume products possible
• Good fatigue strength

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PA 6-G
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183-1
Moisture Absorption at Equilibrium 2.2 %
@Temperature 23.0 °C
50% RH
Water Absorption at Saturation 6.5 %
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 88dry; ISO 2039-2
Hardness, Shore D 77DIN 53505
Ball Indentation Hardness 165 MPadry; ISO 2039-1
Tensile Strength, Yield 55.0 MPa50% RH; ISO 527-1
 86.0 MPadry; ISO 527-1
Elongation at Break 25 %dry; ISO 527-1
 >= 50 %50% RH; ISO 527-1
Creep Strength 10.0 MPa
@Time 3.60e+6 sec
stress leading to 1% elongation; 50% RH; ISO 899-1
 22.0 MPa
@Time 3.60e+6 sec
stress leading to 1% elongation; dry; ISO 899-1
Modulus of Elasticity 1.75 GPa50% RH
 3.60 GPadry
Compressive Yield Strength 26.0 MPa
@Strain 1 %
dry; ISO 604
 51.0 MPa
@Strain 2 %
dry; ISO 604
 92.0 MPa
@Strain 5.0 %
dry; ISO 604
Charpy Impact Unnotched NBdry; ISO 179-1/1eU
 NBISO 179
Charpy Impact, Notched 3.50 kJ/m²dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.30
Sand Slurry 0.12µm/km
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+12 ohm-cm50% RH; IEC 60093
 >= 1.00e+14 ohm-cmdry; IEC 60093
Surface Resistance >= 1.00e+12 ohm50% RH; IEC 60093
 >= 1.00e+13 ohmdry; IEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
dry; IEC 60250
 3.6
@Frequency 100 Hz
dry; IEC 60250
 3.7
@Frequency 1e+6 Hz
50% RH; IEC 60250
 6.6
@Frequency 100 Hz
50% RH; IEC 60250
Dielectric Strength 17.0 kV/mm50% RH; IEC 60243-1
 25.0 kV/mmdry; IEC 60243-1
Dielectric Loss Index 0.012
@Frequency 100 Hz
dry; IEC 60250
 0.016
@Frequency 1e+6 Hz
dry; IEC 60250
 0.050
@Frequency 1e+6 Hz
50% RH; IEC 60250
 0.14
@Frequency 100 Hz
50% RH; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 90.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.290 W/m-K
Melting Point 215 °CISO 11357-1
Maximum Service Temperature, Air 90.0 °C
@Time 7.20e+7 sec
 105 °C
@Time 1.80e+7 sec
 170 °C
@Time <=86400 sec
Minimum Service Temperature, Air -30.0 °C
Glass Transition Temp, Tg 50.0 °CISO 11357-1
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorNatural/Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12
Overview of materials for Nylon 6, Cast
Aclo Accucomp Nylon 6 NY0700L
Cast Nylons Nycast® 12 Cast Nylon 12
Akro-Plastic Akromid® B3 (2500) PA 6 Dry

PMURT924 / 156571

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.