MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Tenite™ Renew Propionate 383A4000011 Clear Trsp - 24 Cellulosic Plastics
Categories: Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Tenite™ Renew cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite™ Renew cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite Renew cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Renew Cellulose Acetate Propionate 383-11 contains a mold release and has a plasticizer level of 11%. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Consumer housewares-nfc
  • Electronic connectors
  • Eyeglass frames
  • Eyewear
  • Flooring
  • Furniture
  • Profiles
  • Small appliances non-food contact

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 1.50 %
@Time 86400 sec
immersion; ASTM D570
Linear Mold Shrinkage 0.00200 - 0.00600 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 81.0ASTM D785
Tensile Strength at Break 34.5 MPaASTM D638
Tensile Strength, Yield 33.3 MPaASTM D638
Elongation at Break 45.0 %ASTM D638
Flexural Yield Strength 43.7 MPaASTM D790
Flexural Modulus 1520 MPaASTM D790
Izod Impact, Notched 103 J/m
@Temperature -40.0 °C
ASTM D256
 353 J/m
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.30 - 3.80
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mmASTM D149
Dissipation Factor 0.0100 - 0.150
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 90.0 µin/in-°FASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C
Thermal Conductivity 0.170 - 0.330 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °CASTM D648
Vicat Softening Point 98.0 °CConditioned 4 hours at 70°C; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46 - 1.49ASTM D542
Haze <= 8.50 %ASTM D1003
Transmission, Visible >= 90.0 %ASTM D1003
 
Descriptive Properties
Content (%)11Plasticizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4180 / 323803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.