MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Tenite™ Renew Propionate 383A4000011 Clear Trsp - 24 Cellulosic Plastics
Categories: Polymer; Thermoplastic; Cellulosic; Cellulose Acetate Propionate, Molded

Material Notes: Tenite™ Renew cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite™ Renew cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite Renew cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Renew Cellulose Acetate Propionate 383-11 contains a mold release and has a plasticizer level of 11%. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Consumer housewares-nfc
  • Electronic connectors
  • Eyeglass frames
  • Eyewear
  • Flooring
  • Furniture
  • Profiles
  • Small appliances non-food contact

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 1.50 %
@Time 86400 sec
1.50 %
@Time 24.0 hour
immersion; ASTM D570
Linear Mold Shrinkage 0.00200 - 0.00600 cm/cm0.00200 - 0.00600 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 81.081.0ASTM D785
Tensile Strength at Break 34.5 MPa5000 psiASTM D638
Tensile Strength, Yield 33.3 MPa4830 psiASTM D638
Elongation at Break 45.0 %45.0 %ASTM D638
Flexural Yield Strength 43.7 MPa6340 psiASTM D790
Flexural Modulus 1.52 GPa220 ksiASTM D790
Izod Impact, Notched  1.03 J/cm
@Temperature -40.0 °C
1.93 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 3.53 J/cm
@Temperature 23.0 °C
6.61 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 - 1.00e+15 ohm-cm1.00e+13 - 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.30 - 3.80
@Frequency 1.00e+6 Hz
3.30 - 3.80
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 11.8 - 18.7 kV/mm300 - 475 kV/inASTM D149
Dissipation Factor 0.0100 - 0.150
@Frequency 1.00e+6 Hz
0.0100 - 0.150
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 108 - 162 µm/m-°C60.0 - 90.0 µin/in-°FASTM D696
Specific Heat Capacity 1.26 - 1.67 J/g-°C0.301 - 0.399 BTU/lb-°F
Thermal Conductivity 0.170 - 0.330 W/m-K1.18 - 2.29 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C169 °FASTM D648
Vicat Softening Point 98.0 °C208 °FConditioned 4 hours at 70°C; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46 - 1.491.46 - 1.49ASTM D542
Haze <= 8.50 %<= 8.50 %ASTM D1003
Transmission, Visible >= 90.0 %>= 90.0 %ASTM D1003
 
Descriptive Properties
Content (%)11Plasticizer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM4180 / 323803

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.