MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Abatron AboCast 8103-11 One Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: One component system. Information provided by Abatron, Inc.

Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At 100°C (212°F), gels in 3-4 hrs, total cure in 4-6 hrs. At 110-120°C (230-250°F) gels to 0.5-1 hr and total cure in 1-2 hrs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 12000
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 111
Tensile Strength, Ultimate 39.0 MPa
Elongation at Break 1.6 %
Flexural Yield Strength 96.53 MPa
Flexural Modulus 3.10 GPa
Compressive Yield Strength 113.8 MPa
Compressive Modulus 2.30 GPa
 330000 psi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 9.63e+15 ohm-cm
Surface Resistance 7.85e+15 ohm
Dielectric Constant 3.15
@Frequency 1e+6 Hz
 3.35
@Frequency 1000 Hz
 3.36
@Frequency 60 Hz
Dissipation Factor 0.0035
@Frequency 60 Hz
 0.055
@Frequency 1000 Hz
 0.23
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °CDeflection temperature; load unknown.
 
Descriptive Properties
Exotherm170°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay LTM® 123 Cyanate Ester for Prepregs
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled
Abatron AboCast 8504-1 One-Component Epoxy

PABEM1 / 22013

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.