MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Abatron AboCast 8103-11 One Part Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: One component system. Information provided by Abatron, Inc.

Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At 100°C (212°F), gels in 3-4 hrs, total cure in 4-6 hrs. At 110-120°C (230-250°F) gels to 0.5-1 hr and total cure in 1-2 hrs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 1200012000
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 111111
Tensile Strength, Ultimate 39.0 MPa5660 psi
Elongation at Break 1.6 %1.6 %
Flexural Yield Strength 96.53 MPa14000 psi
Flexural Modulus 3.10 GPa450 ksi
Compressive Yield Strength 113.8 MPa16510 psi
Compressive Modulus 2.28 GPa330 ksi
 2.30 GPa334 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 9.63e+15 ohm-cm9.63e+15 ohm-cm
Surface Resistance 7.85e+15 ohm7.85e+15 ohm
Dielectric Constant  3.15
@Frequency 1e+6 Hz
3.15
@Frequency 1e+6 Hz
 3.35
@Frequency 1000 Hz
3.35
@Frequency 1000 Hz
 3.36
@Frequency 60 Hz
3.36
@Frequency 60 Hz
Dissipation Factor  0.0035
@Frequency 60 Hz
0.0035
@Frequency 60 Hz
 0.055
@Frequency 1000 Hz
0.055
@Frequency 1000 Hz
 0.23
@Frequency 1e+6 Hz
0.23
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °FDeflection temperature; load unknown.
 
Descriptive Properties
Exotherm170°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay LTM® 123 Cyanate Ester for Prepregs
Overview of materials for Thermoset Polyurethane, Liquid, Quartz Filled
Abatron AboCast 8504-1 One-Component Epoxy

PABEM1 / 22013

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.