MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ethyl Acrylate
Categories: Fluid

Material Notes: Formula: C5H8O2

CAS: 140-88-5

Description: Acrylic acid ester suitable for the production of polymers and as a feedstock for syntheses.

Applications: Ethyl acrylate forms homopolymers and copolymers. Copolymers of ethyl acrylate can be prepared with acrylic acid and its salts, amides and esters, methacrylates, acrylonitrile, maleates, vinyl acetate, vinyl chloride, vinylidene chloride, styrene, butadiene, unsaturated polyesters and drying oils. Ethyl acrylate is also an important feedstock for chemical syntheses because it readily undergoes addition reactions with many organic and inorganic compounds.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.922 g/cc
Viscosity 0.55 cP
Molecular Weight 100.1 g/mol
Vapor Pressure 0.00390 bar
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.98 J/g-°Cof Liquid
Melting Point -72.0 °CFreezing Point
Boiling Point 100 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.404
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %ASTM D203
 
Descriptive Properties
Assay>99.7%
Color<10APHA, ASTM D1209
Heat of Polymerization655 kJ/kg
Latent Heat of Evaporation at Boiling Point346.1 kJ/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ecoflex® F BX 7011 Biodegradable Plastic
BASF Butyl Acrylate
Dow Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Overview of materials for Methacrylate Adhesive
Overview of materials for Acrylic, General Purpose, Molded

PBASG0959 / 132592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.